WoodHighly absorbent

Data source

PTB reference data

Physikalisch-Technische Bundesanstalt

Source: DNA 1968, Tabelle a3.1-6

Value from the PTB table, not verified

Lightweight chipboard on cross-battening (DNA 1968, a3.1-6)

PTB reference data

Original description

Lightweight chipboard on cross-battening (DNA 1968, a3.1-6)

Material properties

Thickness: 0.7 in
Wall distance: 2 in
Surface weight: 5.7 kg/m²
Flow resistance: 55 Rayl
Mounting: cross-battening 24/1.9 in

Measurement data

Sound absorption

Reverberation chamber (ASTM C423 / ISO 354)

NRC
0.65
derived from ISO 354 lab data

Frequency values

αp nach ISO 11654

f (Hz)1252505001k2k4k
αp0.150.450.850.650.650.60

Create a permanent free accountAccess frequency bands, variants and export.

Free. No password required.

Value from the PTB table, not verified

NRC: 0.65 (derived from ISO 354 lab data)

Terms of use
Measured values as a table (1 measurement)
Lightweight chipboard on cross-battening (DNA 1968, a3.1-6): sound absorption coefficient αs per ISO 354 by frequency and test build-up
Build-upNRC100 Hz125 Hz160 Hz200 Hz250 Hz315 Hz400 Hz500 Hz630 Hz800 Hz1000 Hz1250 Hz1600 Hz2000 Hz2500 Hz3150 Hz4000 Hz5000 Hz6300 Hz
19 mm · 5,7 kg / m^2 · 50 mm · Montiert on Kreuzlattung 24/48 mm, Air cavity 50 mm, horizontaler Abstand 800 mm, vertikaler Abstand 625 mm, Ränder der Prüffläche seitlich geschlossen0.650.080.120.190.260.420.600.800.860.830.730.670.600.580.650.720.700.560.570.67
Measured values as a table (1 measurement)

Access frequency bands, variants and export. Create a permanent free account